Long term microstructural stability of intermetallic Ti-46Al-8Ta alloy during ageing at temperatures of 700-800 °C LAPIN, J., PELACHOVA, T., STANEKOVA, H., DOMANKOVA, M. Key words: titanium aluminides, TiAl, phase identification, microstructure, diffraction vol. 48 (2010), no. 6, pp. 337 - 343 DOI: 10.4149/km_2010_6_337 Article | Full Text (509 kB)Prediction of fracture toughness temperature dependance from tensile test parameters SMIDA, T., BABJAK, J., DLOUHY, I. Key words: steels, brittle to ductile transition, fracture, toughness, artificial neural network vol. 48 (2010), no. 6, pp. 345 - 352 DOI: 10.4149/km_2010_6_345 Article | Full Text (261 kB) Influence of Sb and Cu in Sn-Sb-Cu alloys on wetting of Cu and Cu-solder-Cu joint strength SEBO, P., SVEC, P., JANICKOVIC, D., ILLEKOVA, E. Key words: lead-free solder, antimony, wetting, Cu-solder-Cu strength vol. 48 (2010), no. 6, pp. 353 - 359 DOI: 10.4149/km_2010_6_353 Article | Full Text (335 kB) Lead zirconate titanate films prepared by liquid source misted chemical deposition KOVAL, V., BHARADWAJA, S. S. N., TROLIER-MCKINSTRY, S. Key words: ferroelectric, thin film, PZT, misted deposition, dielectric properties vol. 48 (2010), no. 6, pp. 361 - 365 DOI: 10.4149/km_2010_6_361 Article | Full Text (166 kB) Influence of scatter of cyclic properties of material on operational endurance of construction KLIMAN, V., KEPKA, M., VACLAVIK, J. Key words: material’s cyclic properties, fatigue-life distribution function, probabilistic analysis, welded joint vol. 48 (2010), no. 6, pp. 367 - 378 DOI: 10.4149/km_2010_6_367 Article | Full Text (385 kB) Characterization of carbon nanofibers by SEM, TEM, ESCA and raman spectroscopy TATARKO, P., PUCHY, V., DUSZA, J., MORGIEL, J., BASTL, Z., MIHALY, J. Key words: carbon micro/nanofiber, cylindrical fiber, bamboo-shaped fiber vol. 48 (2010), no. 6, pp. 379 - 386 DOI: 10.4149/km_2010_6_379 Article | Full Text (395 kB)
Info: 6 records found. |